410/HT stainless steel
C | Mn | Si | P | S | Cr | Ni |
0.15 | 1.00 | 1.00 | 0.04 | 0.03 | 11.5-13.5 | 0.50 |
Tensile Strength MPa (min) | Yield Strength 0.2% MPa(min) | Elongation (% in 50mm) min | Hardness (Rockwell B) MAX |
450 | 205 | 20 | 96 |
Density lbm/in3 |
Thermal Conductivity (BTU/h ft. °F) |
Electrical Resistivity (in x 10-6) |
Modulus of Elasticity (psi x 106 |
Coefficient of Thermal Expansion (in/in)/ °F x 10-6 |
Specific Heat (BTU/lb/ °F) |
Melting Range (°F) |
at 68°F: 0.280 | 187 at 212°F | 23.7 at 68°F | 29 | 6.0 at 32 – 212°F | 0.11 at 68°F to 212°F | 2700 to 2790 |
Alloy 410HT is the basic, general purpose, heat treated version of Type 410. It is a martensitic type, used for general purpose, where corrosion is not severe. Alloy 410 contains a minimum of 11.5% chromium which is just sufficient enough to demonstrate corrosion resistance properties in mild atmospheres, steam, and many mild chemical environments.
Applications requiring moderate corrosion resistance and high mechanical properties are ideal for Alloy 410HT. Examples of applications that frequently used Alloy 410HT include:
- Cutlery
- Steam and gas turbine blades
- Kitchen utensils
- Bolts, nuts, screws
- Pump and valve parts and shafts
- Mine ladder rugs
- Dental and surgical instruments
- Nozzles
- Hardened steel balls and seats for oil well pumps
- NM400 steel plate
- low alloy steel plate
- Cor-Ten steel plate
- stainless steel plate
- pipeline steel plate
- pressure vessel steel plate
- abrasion resistant steel plate
- shipbuilding steel plate
- steel coil
- carbon steel plate
- Cold rolled steel coil
- testing
- quality policy Steel Grades
- EN 10130 cold rolled steel coil specification
- GB/T5213 - 2008 cold rolled coil
- JIS G3141 steel coil specification
- NM500 wear resistant steel
- NM450 wear resistant steel